Metal Radar™: inside the measuring cavity
Metallization in a minute.
A 2.45 GHz cylindrical cavity, about 10 cm across, with the sample in a ceramic tube on its axis where the electric field is strongest. Watch one measuring cycle: empty-cavity reference, filling, compaction by the inverted-T ram, nitrogen purge, a sweep across the resonance, the result, and discharge.
Step:—
- The empty-cavity reference (sharp grey peak) is measured between samples to correct for drift and detect fouling.
- With the sample in place, oxide stores and absorbs field energy, so the resonance moves lower and broadens; metallic iron conducts and shields, changing the shift and Q differently.
- Shift and Q, with the measured mass, compacted height and temperature, give metallization.